Silastic Q7 4765 Biomedical Grade ETR Elastomer, Kit |
![](../images/col_uses.gif) |
Two-part, platinum-catalyzed (1:1 by weight), enhanced tear-resistant silicone elastomers. SILASTIC BioMedical Grade ETR Elastomers (Q7-4720, Q7-4735, Q7-4750, Q7-4765, Q7-4780) are heat-cured elastomers designed for fabricating devices for the healthcare industry. These elastomers are strained through a 200-mesh (75-micron) or finer screen to remove particulate contamination. |
![](../images/col_property.gif) |
Durometer Hardness, Shore A: 63 Tensile Strength, Die C: 7.9 MPa (1150 psi) Elongation: 920% Tear Strength, Die B: 46.5 kg/cm (260 ppi) Relative Density: 1.20 |
|
|