EXXONMOBIL PP 1572 |
![](../images/col_chem_composition.gif) |
Homopolymer |
![](../images/col_uses.gif) |
Homopolymer resin for compression molding applications. |
![](../images/col_property.gif) |
Melt Flow Rate (230'C/2.16 kg): 2.1 g/10 min Density 0.90 g/cm 3 Tensile Strength @ Yield (2 in/min, 50 mm/min): 5.5 kpsi 38 MPa Flexural Modulus, 1% Secant (0.05 in/min, 1.3 mm/min): 276 kpsi 1903 MPa Izod Impact Strength Notched, @ 23'C (73'F): 1.0 ft-lb/in 53 J/m Heat Deflection Temperature @ 66 psi, 455 kPa: 252'F 122'C Typical Processing Temperature 400-455'F 204-235'C |
|
|